Incoloy 330





Lork Group high-quality Incoloy 330 (UNS N08330; W. Nr. 1.4886) is an austenitic alloy with good high-temperature strength and corrosion resistance. It has a solid solution composition and is not hardenable by heat treatment.
Lork Group high-quality Incoloy 330 (UNS N08330; W. Nr. 1.4886) is an austenitic alloy with good high-temperature strength and corrosion resistance. It has a solid solution composition and is not hardenable by heat treatment.
Its high nickel and chromium provide good resistance to oxidation and carburization. Its oxidation resistance is enhanced by the silicon content. The alloy's strength and oxidation resistance at elevated temperatures make it a useful material for industrial heating furnaces; for muffles, retorts, conveyor systems, baskets and boxes, and various fixtures.
Incoloy 330 is also known for its good fabricability, including excellent weldability and formability. This allows it to be easily shaped and joined, making it a versatile material for a variety of manufacturing processes.
AMS 5592, ASTM B536
AMS 5716
ASTM B511
ASTM B535
ASTM B546
ASTM B710
|
|
|
|
|
43 |
|
|
34-37 |
|
|
17-20 |
|
|
<=2 |
|
|
|
|
|
|
|
8.08 gm/cm3 |
0.292 lb/in3 |
|
|
|
|
|
|
600 MPa |
87 ksi |
|
|
280 MPa |
40.6 ksi |
|
|
45% |
45% |